Figure (a) TEM micrographs of the Al-Ti-Fe-Cr RS P/M alloy annealed at 573 K for 1000 h. SAED patterns taken from (b) icosahedral, (c) both icosahedral and a-Al, and (d) a-Al phases. Diffraction spots are indexed by an fcc Al crystal.